Preservative substances and hydrophobizators for wood and concrete,
automobile chemical goods, paint removers, anticorrosive PM, solvents for printing industry.

Hydrofobization and surface stabilization

Summary Table of Base Hydrophobizators and Stabilizers Properties

Compositions/components Base Hydrofuge-1 Base Hydrofuge-8 Base Hydrofuge-10
Plaster Stabilizer
Base Hydrofuge-15
Gypsum Stabilizer
Effect Hydrofobization, stabilization, constructive surface protection from salt efflorescence and biodeterioration
Construction surface Brick,
brick with subsequent filling,
granite,
camstone,
terazzite plaster
foamed concrete,
gas concrete,
sawdust concrete
Lime plaster, terazzite plaster, camstone,
silica brick
Lime plaster, terazzite plaster, red brick with subsequent filling,
lime-based leveling compositions,
concrete-based leveling compositions
Gypsum,
foamed concrete,
gas concrete,
CBPB
Special features Working on a base surface with residual moisture is possible For dry surfaces only
“Wet stone” effect (color intensification) yes no
Application frequency Double Till enriched
Application method Spray diffuser, roller or brush.
Use wet-on-wet or wet-on-dry technology according to the consumption rate
Consumption rate Brick — minimum 150-200 ml/sq m;
brick with subsequent filling — minimum 150-200 ml/sq m;
granite — minimum 75-100 ml/sq m;
camstone — minimum 200-250 ml/sq m;
plaster — minimum 200-250 ml/sq m;
foamed concrete — minimum 400 ml/sq m;
gas concrete — minimum 400 ml/sq m;
sawdust concrete — minimum 400 ml/sq m
foamed concrete — minimum 400 ml/sq m;
gas concrete — minimum 400 ml/sq m;
sawdust concrete — minimum 400 ml/sq m
Lime plaster — minimum 350 ml/sq m;
terazzite plaster — minimum 350 ml/sq m;
camstone — minimum 200 ml/sq m;
silica brick — minimum 300 ml/sq m;
Lime plaster — minimum 400 ml/sq m;
terazzite plaster — minimum 400 ml/sq m;
red brick with subsequent filling — minimum 200 ml/sq m;
lime based leveling compositions — minimum 250-300 ml/sq m;
concrete based leveling compositions — minimum 250-300 ml/sq m
Gypsum — minimum 300 ml/sq m;
foamed concrete — minimum 250-300 ml/sq m;
gas concrete — minimum 250-300 ml/sq m;
CBPB — minimum 250-300 ml/sq m
Repainting possibility Yes, it is required to wash a surface with a professional cleaning composition FAS-101 Yes, once it dries out, the treated surface is ready for painting